[1]
|
Mallory, G.O. and Hadju, J.B. (1991), “Electroless Plating: Fundamentals and
Applications”, AESF, Orlando.
|
[2]
|
Riedel, W. (1991), “Eletroless nickel plating. Stevenage”, Finishing Publications Ltd.,
Hertfordshire, UK.
|
[3]
|
Agarwala, R.C. and Agarwala, V. (2003), “Electroless alloy/composite coatings: A
review”, Sadhana 28(3-4), pp. 475-493.
|
[4]
|
Sahoo, P. and Pal, S.K. (2007), “Tribological performance optimization of electroless
Ni-P coatings using the Taguchi method and grey relational analysis”, Tribol Lett 28(2),
pp. 191-201.
|
[5]
|
Sahoo, P. and Das, S.K. (2011), “Tribology of electroless nickel coatings - A review”,
Mater Des 32, pp. 1760-1775.
|
[6]
|
Narayanan, T.S.N.S., Krishnaveni, K. and Seshadri, S.K. (2003), “Electroless Ni-P/Ni-
B duplex coatings: Preparation and evaluation of microhardness, wear and corrosion
resistance”, Mater Chem Phys 82(3), pp. 771-779.
|
[7]
|
Kanta, A.F., Vitry, V. and Delaunois, F. (2009), “Wear and corrosion resistance
behaviours of autocatalytic electroless plating”, J Alloys Compd 486(1-2), pp. L21-23.
|
[8]
|
Delaunois. F. and Lienard, P. (2002), “Heat treatments for electroless nickel-boron
plating on aluminium alloys”, Surf Coat Technol 160(2-3), pp. 239-248.
|
[9]
|
Srinivasan, K.N., Meenakshi, R. and Santhi, A., Thangavelu, P.R. and John, S. (2010),
“Studies on development of electroless Ni-B bath for corrosion resistance and wear
resistance applications”, Surf Eng 26(3), pp. 153-158.
|
[10]
|
Narayanan, T.S.N.S. and Seshadri, S.K. (2004), “Formation and characterization of
borohydride reduced electroless nickel deposits”, J Alloys Compd 365(1-2), pp. 197-
205.
|
[11]
|
Dervos, C.T., Novakovic, J. and Vassiliou, P. (2004), “Vacuum heat treatment of
electroless Ni-B coatings”, Mater Lett 58(5), pp. 619-623.
|
[12]
|
Anik, M., Korpe, E. and Sen, E. (2008), “Effect of coating bath composition on the
properties of electroless nickel-boron films”, Surf Coat Technol 202(9), pp. 1718-1727.
|
[13]
|
Contreras, A., León, C., Jimenez, O., Sosa, E. and Pérez, R. (2006), “Electrochemical
behavior and microstructural characterization of 1026 Ni-B coated steel”, Appl Surf Sci
253(2), pp. 592-599.
|
[14]
|
Taguchi, G. (1990), “Introduction to Quality Engineering”, Asian Productivity
Organization, Tokyo.
|
[15]
|
Ross, P.J. (1996), “Taguchi Techniques for Quality Engineering”, 2nd edn., McGraw
Hill, New York.
|
[16]
|
Roy, R.K. (1990), “A primer on the Taguchi method”, Society of Manufacturing
Engineers, Dearborn, Michigan.
|
[17]
|
Deng, J. (1989), “Introduction to grey system”, Journal of Grey System 1(1), pp. 1-24.
|
[18]
|
Montgomery, D.C. (2001), “Design and Analysis of Experiments”, Wiley, New York.
|
[19]
|
Cheong, W.J., Luan, B.L. and Shoesmith, D.W. (2007), “Protective coating on Mg
AZ91D alloy - The effect of electroless nickel (EN) bath stabilizers on corrosion
behaviour of Ni-P deposit”, Corros Sci 49(4), pp. 1777-1798.
|
[20]
|
Poorqasemi, E., Abootalebi, O., Peikari, M. and Haqdar, F. (2009), “Investigating
accuracy of the Tafel extrapolation method in HCl solutions”, Corros Sci 51, pp. 1043-
1054.
|
[21]
|
Watanabe, T. and Tanabe, Y. (1976), “Formation and morphology of Ni-B amorphous
alloy deposited by electroless plating”, Materials Science and Engineering 23, pp. 97-
100.
|
[22]
|
Minitab User Manual (2001), “Making data analysis easier”, MINITAB Inc., State
College, PA, USA.
|
[23]
|
Kanta, A.F., Poelman, M., Vitry, V. and Delaunois, F. (2010), “Nickel-boron
electrochemical properties investigations”, J Alloys Compd 505, pp. 151-156.
|
[24]
|
Crobu, M., Scorciapino, A., Elsener, B. and Rossi, A. (2008), “The corrosion resistance
of electroless deposited nano-crystalline Ni-P alloys”, Electrochim Acta 53(8), pp.
3364-3370.
|