Significance of Alloying Element Levels in Realizing the Specified Tensile Properties in 18 Wt % Nickel Maraging Steel

HTML  Download Download as PDF (Size: 344KB)  PP. 1116-1120  
DOI: 10.4236/msa.2011.28150    6,772 Downloads   13,971 Views  Citations

Affiliation(s)

.

ABSTRACT

Among the various grades of commercially available 18 wt. % nickel maraging steels, the one with nominal 0.2% proof strength in the range 1700-1750 MPa is the most commonly used and is distinguished by an excellent combination of high strength and high fracture toughness. The main alloying elements are nickel, cobalt, molybdenum and titanium. The first three of these are present at relatively high concentrations in the chemical composition. The high cost of these metals leads to a high cost of production and this becomes a deterrent to extensive use of the steel. In the present study, an attempt was made to produce the steel by pegging the levels of these alloying elements in the lower half of the specified range. The objective was to save on the raw material cost, while still conforming to the specification. The steel so produced could not, however, attain the specified tensile properties after final heat treatment. The observed behavior is explained based on the role played by the different alloying elements in driving the precipitation hardening reaction.

Share and Cite:

M. Rao and K. Sivasubramanian, "Significance of Alloying Element Levels in Realizing the Specified Tensile Properties in 18 Wt % Nickel Maraging Steel," Materials Sciences and Applications, Vol. 2 No. 8, 2011, pp. 1116-1120. doi: 10.4236/msa.2011.28150.

Copyright © 2024 by authors and Scientific Research Publishing Inc.

Creative Commons License

This work and the related PDF file are licensed under a Creative Commons Attribution 4.0 International License.